Protection against high temperature corrosion with laser welded claddings - Applied and tested on exhaust valve discs of large diesel engines burning heavy fuel oil

2002 ◽  
Vol 53 (2) ◽  
pp. 103-110 ◽  
Author(s):  
D. Schlager ◽  
C. Theiler ◽  
H. Kohn
Author(s):  
Jean-Pierre Stalder ◽  
Peter A. Huber

The use of “clean” fuel is a prerequisite at today’s elevated gas turbine firing temperature, modern engines are more sensitive to high temperature corrosion if there are impurities present in the fuel and/or in the combustion air. It is a common belief that distillate grade fuels are contaminant-free, which is often not true. Frequently operators burning distillates ignore the fuel quality as a possible source of difficulties. This matter being also of concern in plants mainly operated on natural gas and where distillate fuel oil is the back-up fuel. Distillates may contain water, dirt and often trace metals such as sodium, vanadium and lead which can cause severe damages to the gas turbines. Sodium being very often introduced through contamination with seawater during the fuel storage and delivery chain to the plant, and in combination, or with air borne salt ingested by the combustion air. Excursions of sodium in treated crude or heavy fuel oil can occur during unnoticed malfunctions of the fuel treatment plant, when changing the heavy fuel provenience without centrifuge adjustment, or by inadequate fuel handling. For burning heavy fuel, treatment with oil-soluble magnesium fuel additive is state of the art to inhibit hot corrosion caused by vanadium. Air borne salts, sodium, potassium and lead contaminated distillates, gaseous fuels, washed and unwashed crude and residual oil can not be handled by simple magnesium based additives. The addition of elements like silicon and/or chromium is highly effective in reducing turbine blade hot corrosion and hot section fouling. This paper describes field experience with the use of chromium containing fuel additive to reduce high temperature corrosion of hot section parts, as well as the interaction of oil-soluble chromium and magnesium-chromium additives on material behaviour of blades and vanes, and their economical and environmental aspects.


CORROSION ◽  
2001 ◽  
Vol 57 (6) ◽  
pp. 489-496 ◽  
Author(s):  
M. Amaya ◽  
J. Porcayo-Calderon ◽  
L. Martinez

Abstract The performance of Fe-Si coatings and an iron aluminide (FeAl) intermetallic alloy (FeAl40at%+0.1at%B+10vol%Al2O3) in molten salts containing vanadium pentoxide (V2O5) and sodium sulfate (Na2SO4) is reported. Corrosion and fouling by ash deposits containing V2O5 and Na2SO4 are typical corrosion problems in fuel oil-fired electric power units. High-temperature corrosion tests were performed using both electrochemical polarization and immersion techniques. The temperature interval of this study was 600°C to 900°C, and the molten salts were 80wt%V2O5-20wt%Na2SO4. Curves of corrosion current density vs temperature obtained by the potentiodynamic studies are reported, as well as the weight loss vs temperature curves from molten salt immersion tests. Both Fe-Si coatings and FeAl40at%+0.1at%B+10vol%Al2O3 showed good behavior against molten salt corrosion. The final results show the potential of these coatings and alloys to solve the high-temperature corrosion in fuel oil-fired electric power units.


2010 ◽  
Vol 41 (12) ◽  
pp. 1143-1151 ◽  
Author(s):  
Zhongqing Zheng ◽  
Xiaochen Tang ◽  
Akua Asa-Awuku ◽  
Heejung S. Jung

Fuel ◽  
2014 ◽  
Vol 115 ◽  
pp. 145-153 ◽  
Author(s):  
Nikolaos Stamoudis ◽  
Christos Chryssakis ◽  
Lambros Kaiktsis

Sign in / Sign up

Export Citation Format

Share Document